PREFIX=/usr SHAREDIR=$(PREFIX)/share/models PRINT_TEMP=220 PRINT_BED_TEMP=65 PRINT_NOZZLE_DIAM=0.2 PRINT_FILA_DIAM=1.75 # settings for Bambu p1p 3d printer # 50mm/sec w/ raft=2, 0.4diam (wrong!), density 20%: works but causes very rough edges # 40mm/sec w/ raft=0, 0.4diam (wrong!), density 20%: fails; infill becomes too sparse # 35mm/sec w/ raft=0, 0.4diam (wrong!), density 50%, honeycomb: works, corners are rough # 25mm/sec w/ raft=0, 0.2diam, density 75%, rectilinear: fails; detached from bed # 35mm/sec w/ raft=0, 0.2diam, density 75%, rectilinear, first-layer 0.2: works, but takes like 6 hours to print # - 2.5mm thickness => needlessly thick; stiff # - 160mm length => too short # - 3/3.5/6.0mm overhang => too much (that amount of overhang can't be printed reliably) # - port cutouts => should extend into more z PRINT_SPEED=40 PRINT_DENSITY=20 PRINT_RAFT_LAYERS=0 PRINT_FILL_PATTERN=rectilinear # XXX: Slic3r doesn't always set the bed temperature correctly. fix by specifying it also for the first layer. SLIC3R_FLAGS=\ --temperature $(PRINT_TEMP) \ --first-layer-temperature $(PRINT_TEMP) \ --bed-temperature $(PRINT_BED_TEMP) \ --first-layer-bed-temperature $(PRINT_BED_TEMP) \ --nozzle-diameter $(PRINT_NOZZLE_DIAM) \ --filament-diameter $(PRINT_FILA_DIAM) \ --solid-infill-speed $(PRINT_SPEED) \ --first-layer-speed $(PRINT_SPEED) \ --infill-speed $(PRINT_SPEED) \ --raft-layers $(PRINT_RAFT_LAYERS) \ --fill-density $(PRINT_DENSITY) \ --fill-pattern $(PRINT_FILL_PATTERN) \ --use-firmware-retraction \ --first-layer-height 0.2 \ --skirts 2 all: build/cases/pp.stl build/cases/pp.gcode build/cases/pp.stl: src/pp/*.scad build/%.stl: src/%.scad src/*.scad src/lib/*.scad mkdir -p $(shell dirname $@) openscad $< -o $@ %.gcode: %.stl slic3r $(SLIC3R_FLAGS) $< -o $@ install: mkdir -p $(SHAREDIR) install -m644 build/case.stl $(SHAREDIR) install -m644 build/case.gcode $(SHAREDIR) .PHONY: all install